Tabiiy fanlar

PHYSICAL BASIS OF FORMATION OF LAYERED NANO FIBERS MATERIALS AND COMPOSITE COATINGS

electrospinning, electrolysis, composite coating, macroion, biopolymer.

Authors

  • Jaxongir XAQQULOV O‘zbekiston Milliy universiteti fizika-matematika fanlari bo‘yicha falsafa doktori (PhD), Uzbekistan
  • Umar ABDURAHMONOV O‘zbekiston Milliy universiteti professori, f-m.f.d, Uzbekistan
  • Zokir TEMIROV O‘zbekiston Milliy universiteti o‘qituvchisi, Uzbekistan
  • Anvar SULTONOV O‘zbekiston Milliy universiteti magistranti, Uzbekistan

Using the electrospinning device, the optimal conditions for obtaining nanofibers from a 10% solution of Co-AN were
selected, according to which a 25 kV voltage was applied to the filler (< 1 mm), i.e., the anode, installed in the solution
reservoir syringe, and such a voltage was under the cover, nanofibers were formed at a distance of 12-15 cm from the filter to
the screen (cathode).
The electrolysis process was carried out for 4-14 hours at I = 2 mA, I = 4 mA and I = 8 mA. At 4 mA and 8 mA, macroions
were restored on the surface of the electrodes, and their amount was 65-70% of the macroions in the solution.